SailNet Community - Reply to Topic
Thread: bristol coating instead of varnish Reply to Thread
Send Trackbacks to (Separate multiple URLs with spaces) :
Post Icons
You may choose an icon for your message from the following list:

Register Now

In order to be able to post messages on the SailNet Community forums, you must first register.
Please enter your desired user name, your email address and other required details in the form below.
Please note: After entering 3 characters a list of Usernames already in use will appear and the list will disappear once a valid Username is entered.

User Name:
Please enter a password for your user account. Note that passwords are case-sensitive.


Confirm Password:
Email Address
Please enter a valid email address for yourself.

Email Address:


Human Verification

In order to verify that you are a human and not a spam bot, please enter the answer into the following box below based on the instructions contained in the graphic.

  Additional Options
Miscellaneous Options

Click here to view the posting rules you are bound to when clicking the
'Submit Reply' button below

  Topic Review (Newest First)
03-19-2010 09:51 AM
awatson Wanted to post my experience with Bristol finish. I applied several coats, and then carefully stored the remainder of the unmixed product as directed for a few months, and to my dismay, the catalyst had hardened and was ruined. Since I did exactly what I was supposed to, I contacted the manufacturer, as I had lost a significant quantity. They would NOT stand behind their product, and credit me for the additional catalyst, that I now have to purchase.
The jury is still out on how the finish itself performs, but it really needs to deliver, after this setback, in order to earn my recommendation.
12-04-2002 08:45 AM
bristol coating instead of varnish

If you didn''t use so much sailkote on everything the Bristol Finish might stick to the teak!
12-04-2002 08:19 AM
bristol coating instead of varnish

Last year (spring 2001) I scraped off the many layers of Cetol on my exterior teak and applied the recommended 6 coats of Bristol Finish. After about 3 months, it started lifting up at the hard edges of the toe rail -- the 90 degree bend where the top and sides meet. I called the outfit for advice, and talked to the owner. He said it won''t stick to hard bends like that, and that I had to round off the edges if I expected the BF to stick. I wasn''t happy because the literature said nothing about that, and the stuff costs $50 a quart.

So this spring I rounded off the edges as he advised using a random orbital sander (just a tad - not too much) and gave it all another 6 coats of BF. It is holding up very well, although there are a couple of spots where I need to do some more sanding to round it off more.

All told, I am pleased with the final result but wish the literature covered this hard edge issue. BF is a hard, tough finish that looks terrific. My hatch boards look terrific and this was their second full season with the original 6 coats. And I think the toe rails will be fine with the edge rounded off some. When I touch up the couple of spots that need it, I''ll put another 3 coats or so on the toe rails just to be safe, and because I should have enough BF left to do that. May as well use it up on the assumption that it should last another 3-4 years here on the Chesapeake, and I''ll buy new down the road.

12-04-2002 07:37 AM
bristol coating instead of varnish

I have used bristol on my C&C 35 in the great lakes. What is nice about it is you can apply many coats in short amount of time. We did the outside handrails,dorade boxes and hatchway a couple years ago and it has held up very nicely. THis year we roughed it up a bit and applied a another coat.
11-29-2002 02:41 PM
bristol coating instead of varnish

I saw an ad in CW for a product called Bristol finish. I went to their web site and was attracted by the claims of durability.

I had maintained the teak on my norsea 27 for 15 years using Goldspar epiglas varnish from New Zealand. It seemed to hold up better than many other varnishes but now I cant find a source.

So, I have two questions; 1. Does anyone have any experience with this bristol finish?
2. Does anyone know a source of Goldspar epiglas..

Posting Rules  
You may post new threads
You may post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is On

For the best viewing experience please update your browser to Google Chrome